Brand Name :New Era
Model Number :ASTM A179/ SA179
Certification :ISO9001
Place of Origin :China
MOQ :1 tons
Price :Negotiation
Payment Terms :T/T
Supply Ability :3000 tons/month
Delivery Time :45 days
Packaging Details :Bundles Package, Wooden Box Package
Standard :ASTM A179/A179M, ASME SA-179/SA-179M
Similar Materials :Low carbon steel Steel 10; St35.8; E235; St37
Materials :Low carbon material
Size Range :OD:6-127mm,Wt:1-12mm
Application :Low Temperature heat exchanger and condenser tubes
Tubes & Pipes :Cold Drawn
Heat-treatment :Annealed Heat-treatment
Wall Thickness :Minimum Wall Thickness
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

SA179 Seamless Cold Drawn Low Carbon Steel Heat Exchanger and Condenser Tubes

1.This specification covers minimum-wall-thickness,seamless cold-drawn low-carbon steel tubes for tubular
heat exchangers, condensers tubes, and similar heat transfer apparatus.
2.This specification SA179/A179 covers seamless tubes 1⁄8 to 3 in. [3.2 to 76.2 mm], inclusive, in outside diameter.

3.The referenced Documents : A450/A450M Specification for General Requirements for Carbon, Ferritic Alloy, and

Austenitic Alloy Steel Tubes

4.Seamless tubes shall be made by the seamless process and shall be cold drawn tubes.
5.Heat-treatment of Steel tubes shall be heat treated after the final cold draw pass at a temperature of 1200°F [650°C] or higher.

6.Surface of cold drawn steel tubes:Finished tubes shall be free of scale. A slight amount of oxidation will not be considered as scale.

7.Hardness:The tubes shall have a hardness number not exceeding 72 HRB.

8.Mechanical Tests Required:

1) Flattening Test—One flattening test shall be made on specimens from each of two tubes from each lot (Note 2) or fraction thereof.
2) Flaring Test—One flaring test shall be made on specimens from each of two tubes from each lot (Note 2) or fraction thereof.
3) Flange Test—When specified as a substitute for the flaring test, for tubes having a wall thickness (actual mean wall) less than 10 %

of the outside diameter, one test shall be made on specimens from each of two tubes from each lot (Note2) or fraction thereof. For tubes

other than specified above, the flange test shall not be required.


Chemical Composition and Size Tolerance:

Chemical CompositionCMn

P

S

Si

0.06--0.180.27--0.630.0350.0350.25
OD Inch(mm)+--WT Inch(mm)+--
<1(25.4)0.100.10≤1. 1/2 (38.1)20%0

1 to 4

(25.4 to 101.60)

0.150.15>1. 1/222%0

SA179 SMLS Seamless Tube For Heat ExchangerSA179 SMLS Seamless Tube For Heat Exchanger

Tags: ASTM A179, SA179, Heat exchanger tubes, Steel Tube, Seamless Boiler Tube






Inquiry Cart 0